Is there an easy way to identify the year of manufacture of a head (J270316) and base (12/BP 248780) by these serial numbers?



Thanks in advance Scott


Well, a long time ago I copied a fragment of a serial number table from this NG or from the Web or somewhere. Your base, anyway, was made in 1987.

GWE

Think it's in the dropbox, Grant.

Machine builders of new england was mentioned in a recent thread. Among other things, they have a handy little reference for serial numbers to date ranges...