How many layers of oil paint

Feb 09, 2010 25 Replies

Also especially with epoxy paints the surface has to be clean, very clean. Do not use silicon spray cans anywhere around the machine after you prep it for painting. The silicon spray lubricants will cause the paint not to bond properly. The sprays can travel a great distance in the air.

When I paint my machines I use a spray sandable primer surfacer aerosol can. The local surplus place sells some real good spray paint for a buck a can. It covers a lot of chips and scratches. I usually use an alcoyd paint for the top coat. The last couple machines I just used the spray can and then touched up the lettering, handles and misc, levers with a paint brush and oil based paint. Of course all my machines are working commercial shop machines but the spray paint still holds up well and with the spray cans it makes it easy to touch any problem areas.

John

I was assuming spray painting. I think that brush painting would not be as hazardous, unless you move your brush at supersonic speeds. :-) After all -- the problem is inhaling the curing agent, I believe.

Certainly so if you spray -- and probably a good idea even with a brush. But this will give you plenty of time to prime it (as needed for the paint you choose) and let it dry fully. :-)

I'm not sure how thick it would be -- which could be a problem with brush marks brush painting. Of course, with spray, you need to keep in mind the cure time and clean the spray gun well before each batch you mix up gets close to cure. :-)

Good Luck, DoN.

Yes, or "curing agent". The curing action is catalytic polymerization, which converts the resin to a thermoset material. Hence "catalyst" is an appropriate term for what an epoxy hardener is in principle.

Maybe. But we maintain the myth that there is a difference.

Viva la difference!

I happened to meet a couple of Du Pont engineers visiting from Germany. They work for the car paint division. And asked one about painting, specifically about how many coats of primer. He said one coat of primer. But then added that they are in the midst of rolling out the second generation of water based automotive paint. It consists of a base coat with the color and a clear top coat. NO PRIMER.

That sounds pretty neat to me. Automotive paint which ought to stand up to exterior conditions. Just one coat if you don't need a clear coat. And water clean up. Will have to see if I can find out more.