Which carb is on that thing? If it is the Zenith R57 it was VERY common on older tractors and industrial equiment - a fork lift company would likely have the parts available. So would the antique tractor guys. The same basic engine was used in Case V series tractors, Cockshutt 20 and 540 tractors, Oliver Super 44 and 440, Massy 20 series and colt, Co-op, and numerous other tractors. Some were smaller displacement (the 163 was the last of the 4 cyl L Head Contis) If it's a Marvel, parts will be VERY difficult to get hold of, but the Zenith is a bolt-on replacement. If it is an F163 series 4000 Red Seal, most likely it is the Zenith
You can get a lot of information at billswelderrepair.com, and I think they have a lot of parts still available as well.