OT - Foil-back Extruded Styrofoam?

Nov 07, 2011 11 Replies

First reply

Lloyd E. Sponenburgh

"David Courtney" fired this volley in news:j99dcp Lowes in the US carries a two-sided foil-backed EPS (expanded polystrene) bead foam board. I'm unaware of only one-sided foil. It either comes both sides, or none. If you can't find it, consider polyisocyanurate foam, which…

Read the full reply

Is there any foil-backed extruded polystyrene foam insulation available in the US? I've googled & googled and every link leads to Australia or New Zealand; even common product names like "Foamular" only show up with foil "down under" for some reason. I need about 80 to 100 4' x 8' sheets of 2" styrofoam with foil on one side, if I can find it. Any ideas on where to look or what name to search for?


"Foil faced rigid insulation" ? "radiant barrier rigid insulation" ?

Dave

"David Courtney" fired this volley in news:j99dcp $a0t$ snipped-for-privacy@dont-email.me:

Lowes in the US carries a two-sided foil-backed EPS (expanded polystrene) bead foam board. I'm unaware of only one-sided foil. It either comes both sides, or none.

If you can't find it, consider polyisocyanurate foam, which almost always comes foil-backed (both sides, again), and has a higher R-factor per inch than EPS foam. (more resistant to solvents, too! In fact, almost immune to all of them -- nearly as good as polyurethane)

LLoyd

David Courtney Inscribed thus:

Try "Celotex".

Johns Manville AP Foil-faced is one. Think the popularity has waned significantly owing to high oil prices driving it way up in cost.

--

Foil backed urethane foam is common enough in Canada

Thanks for the replies, apparently the answer is "no". Unfortunately, it can't be polyisocyanurate like Johns Manville AP, or "expanded" polystyrene beadboard, or have foil on both sides. Oddly, the blue/pink extruded polystyrene board with foil on one side seems to be popular in Australia & New Zealand but appears to be "unavailable" here; which means I'll be gluing foil or mylar to (probably itself, myself, and) the Pink Panther. >:-(

Thanks for the replies, apparently the answer is "no". Unfortunately, it can't be polyisocyanurate like Johns Manville AP, or "expanded" polystyrene beadboard, or have foil on both sides. Oddly, the blue/pink extruded polystyrene board with foil on one side seems to be popular in Australia & New Zealand but appears to be "unavailable" here; which means I'll be gluing foil or mylar to (probably itself, myself, and) the Pink Panther. >:-(

===================================================================

You probably know this, but be careful about the adhesive you use. A lot of solvents attack polystyrene. You'll want to run a small test first.

I've had good luck using household white glue (Elmer's, PVA). I was surprised that it stuck pretty well to aluminum foil. Use a very thin layer if you do, because it doesn't dry well with aluminum on one side and closed-cell foam on the other.

I'm sure there are better alternatives, but it's cheap, easy to work with, and I already had some. d8-) I did NOT try it on large, household-insulation-type panels. I was just lining a cooler with blueboard for a special purpose.

On 11/8/2011 9:19 AM, David Courtney wrote: ...

OK, inquiring minds and all that...why not? :)

Maybe roll the film out on contact cement or spray adhesive (one surface only should be sufficient, maybe)???

--

ded polystyrene foam insulation available

Depending on the application (and how many panels) and why it has to be that material or only one-sided, maybe the way forwards is to cheat and glue a thin double-sided sheet of the correct (or any) type to a thin sheet of non-foil-backed?

Might be a lot quicker/easier gluing sheets than gluing on foil.

Dave

I'm searching for 8' wide rolls of adhesive-backed foil or reflective film now. It must be kept with the foil-faced polystyrene because I can't find it, either. LOL