Radius slot in O-1

Apr 12, 2006 19 Replies
Jump to replies (19)

Imagine a 1" cube of O-1 with a 1/8" slot milled 9/16 deep through the center of a face. I need to put a 1/16" radius on the two edges on one of the sides. The last one of these I made took hours with itsy-bitsy (technical term) files and emery paper. I have a "Round-over" end mill with a 1/2" radius but I've never seen one that small. Do they exist? I DID Google and looked at catalogs for all the usual mill suppliers. I could make it in two parts but that would be a wash, time wise.


How many do you need to make? Do the rads have to be true and without any sharp edges, or are they only cosmetic? How close to 1/16" do they have to be?

I'd use a die grinder, then stone, then emery cloth/paper. 5 minutes max. start to finish (per rad). This is assuming you cannot find an appropriate radius cutter and/or need a true rad with a good surface finish.

Regards,

Robin

You could take an old end mill, cut away al but one of the flutes then hand grind the 1/16 r in the remaining flute aking it a single point cutter. A little time consuming, but faster than hand work.

A 1/16 round over end mill should be a stock size. I know for a fact that we have about six or 7 of them in our cutter bin at work.

You might be best off just phoning a (relatively) local supplier and asking, but MSC will probably have them.

Lesse.... McMaster Carr item 3067A11 in hss, 2790A71 in cobalt steel. Pg.2249 in cat #107 So these numbers may or may not be any good.

Cheers Trevor Jones

It helps to be looking for something using the right name for it...Duhh. What catalog do you have? I have 111 and 112 and I found the mill but nowhere near your page numbers. (How do you like that, I now get a new catalog from them every year rather than every other year as before...I'm quite impressed with their service and even their prices lately.)

Uhhhh.... That would be cat # 107, same as before.

:-)

Cheers Trevor Jones

I was just testing you to see if you would stick to your story.

According to Tom Gardner :

It sounds to me as though you would do better in cutting the slot with a conventional milling cutter (for a horizontal spindle mill) instead of an endmill, and while we're about it, (assuming that you will be making enough of these to make it worthwhile) you can get another milling cutter a bit wider reground by a good sharpener to produce the radius on both sides at the same time. Perhaps even one could be ground to produce the slot at full depth and both radii in a single pass, so you don't have to be constantly changing cutters.

Good Luck, DoN.

Or build a simple fixture to run both (or all three) cutters at once. If the run was long enough, a fixture could be made to hold multiple parts for each operation. This of course assumes the part would be run on a proper horizontal using an arbour with the ground spacer bushings.

I'm not sure having one cutter for both the slot and the rad would be a great idea. If each rad and the slot are cut individually, all the cutters are probably off-the-shelf. Specially ground cutters are expensive to buy, expensive to sharpen, and expensive to replace in the case of a crash.

Regards,

Robin

I only have to make one Don, and the slot is already done with a cutter. I just need to radius the sides of the slot. The part will be a guide for .110" x .017" flat wire that will be poking into the slot from about a half inch away, very fast. Then the wir gets cut and pulled out...kinda'. The radius is only to keep the cut edges from hanging-up as it gets inserted into the slot in the block and make sure it ends up in position.

It doesn't seem economical to buy any specific tooling for this part if you one need one unit. It sounds like the actual dimension and form of the rad is somewhat unimportant, as long as there is something there to catch your wire.

If I didn't have a die grinder, I'd use a file too. Why did it take 2 hours of bench work last time (perhaps I'm missing something)?

Regards,

Robin

220 0 article Path: finder4.readnews.com!fnd01.iad01.newshosting.com!textbe01-ams!hwmnpeer02.ams!hw-filter.ams!hwmnpeer01.ams!hwmnpeer01.lga!hwmedia!news.highwinds-media.com!news.glorb.com!wn13feed!worldnet.att.net!207.35.177.252!nf3.bellglobal.com!nf1.bellglobal.com!nf2.bellglobal.com!news20.bellglobal.com.POSTED!not-for-mail From: "Robin S." Newsgroups: rec.crafts.metalworking References: Subject: Re: Radius slot in O-1 Lines: 19 X-Priority: 3 X-MSMail-Priority: Normal X-Newsreader: Microsoft Outlook Express 6.00.2900.2670 X-MimeOLE: Produced By Microsoft MimeOLE V6.00.2900.2670 X-RFC2646: Format=Flowed; Response Message-ID: Date: Fri, 14 Apr 2006 20:22:31 -0400 NNTP-Posting-Host: 65.95.149.89 X-Complaints-To: snipped-for-privacy@sympatico.ca X-Trace: news20.bellglobal.com 1145060552 65.95.149.89 (Fri, 14 Apr 2006 20:22:32 EDT) NNTP-Posting-Date: Fri, 14 Apr 2006 20:22:32 EDT Organization: Bell Sympatico Xref: finder4.readnews.com rec.crafts.metalworking:211008 X-Received-Date: Fri, 14 Apr 2006 19:41:00 MST (textbe01-ams)

It doesn't seem economical to buy any specific tooling for this part if you one need one unit. It sounds like the actual dimension and form of the rad is somewhat unimportant, as long as there is something there to catch your wire.

If I didn't have a die grinder, I'd use a file too. Why did it take 2 hours of bench work last time (perhaps I'm missing something)?

Regards,

Robin

According to Tom Gardner :

[ ... ]
[ ... ]

O.K. For that, you could live with a bevel cut with a 90 degree conventional milling cutter doing both sides at once -- or even using a countersink as an end mill. (Yes - I have done that last -- before I had my horizontal mill and some of the interesting cutter shapes.

Enjoy, DoN.

According to Robin S. :

You could even stack the two radius cutters and the slotting cutter to do it all in one pass -- except that the conventional radius cutters which I have seen tend to have a bit too much meat to even go into the 1/8" slot, which is why I was suggesting a custom tool.

Enjoy, DoN.

The slot is only 1/8 and it's hard to get a good swipe at it with the files and the O-1 is tough and I'm lazy and I bore easily. But, the first one has been in service for 18 months and still perfectly smoothe. I'll buy the $34 mill from MC, it's solid carbide and there are two more similar parts I need to make so I can justify it. This machine will make me the largest producer of flat wire brushes in the world! Bwahhahahah!

formatting link

I've heard about you and your "Interesting Shapes"!

...I could use a 90 deg cutter and...maybe I won't spend the$34.

On Fri, 14 Apr 2006 23:44:51 GMT, "Tom Gardner" wrote: If one piece is all that is needed, just dress a concave radius in a wheel, and do the job on a surface grinder.

John Normile

222 87067 body On Fri, 14 Apr 2006 23:44:51 GMT, "Tom Gardner" wrote: If one piece is all that is needed, just dress a concave radius in a wheel, and do the job on a surface grinder.

John Normile

Just buttin in...ever thought of using ceramic wire guides, Tom? Seems to me I saw a guide that was pretty darned close to what you have described at the wire convention in Atlanta a few years back. Unfortunately, the company name eludes me now. With all the various wire guides you use, there may be an off the shelf solution available. Ceramic guides do last one heck of a long time but of course, must me mounted in a steel backer of some sort.

Not exactly right for what you are speaking of but one example for a 10 second search:

formatting link
Koz

I was thinking the same thing, though it sounds like these guides may take a beating, so carbide might be better. I've used both ceramic and carbide eyelets and guides from these folks...

formatting link
I don't see anything there that looks like what I'm imagining from Tom's decription, but they do specials, and delivery isn't too bad.

Ned Simmons

Join the Discussion

Have something to add? Share your thoughts — no account required.

Didn't find your answer?

Ask the community — no account required