Recipe for silly putty

Sep 15, 2003 Last reply: 1 year ago 6 Replies
Jump to replies (6)

I just *had* to pass this on...


And if you back up to:

formatting link
find all kinds of interesting and amusing science games. Regards Dave Mundt

That is ignorant nonsense. Silly Putty is a silicone polymer. The borate is poisonous, letal dose 1 tsp for a child.

Careful, it goes stinky after a few days.

Tim

BOGUS

Here are the real ingrediants of silly putty.

Silicone Bouncing Putty Ingredients Ingredients for Silicone Bouncing Putty (Dow Corning 3179 Dilatant Compound) Percentages by weight.

65% - Dimethyl Siloxane, hydroxy-terminated polymers with boric acid 17% - Silica, quartz crystalline 9% - Thixotrol ST 4% - Polydimethylsiloxane 1% - Decamethyl cyclopentasiloxane 1% - Glycerine 1% - Titanium Dioxide

thanks for sharing real ingradients, need one more help please respond process also if it it is simple mixing ingraients nd mixing at some higher tempreture..

Join the Discussion

Have something to add? Share your thoughts — no account required.

Didn't find your answer?

Ask the community — no account required