-- Geoff
I have some 316 wire - I don't recall off the top what LT-1 means. What size are you looking for and what length ? The roll is in my shop with the 316 steel (to be used as TIG source wire). Martin
Read the full replyDoes anyone have a source for 316LT-1 in something less than a 25 lb spool?
-- Geoff
I have some 316 wire - I don't recall off the top what LT-1 means.
What size are you looking for and what length ?
The roll is in my shop with the 316 steel (to be used as TIG source wire).
Martin
"lionslair at consolidated dot net" wrote in news:42cdf7da$1 snipped-for-privacy@spool9-west.superfeed.net:
It's flux-cored 316. You use it with C25.