Watched tank running day at Bovington (UK) FWIW

Sep 28, 2026 Last reply: 4 weeks ago 22 Replies

I forgot to include the other impediment mentioned. Germany was broaching, not milling, the aforementioned gears. From the above statement I gather that's less than optimum.

-----------------------------------

I believe that depends on how much the final tooth surface has been deformed and possibly cracked by the cutting force. Milling removes thin chips rapidly with little effect on the uncut metal while broaching may be a more brute force bulldozer approach, depending on the tooling and depth of cut. Drilling vs punching illustrate the difference. Milling is like drilling, broaching like punching.

formatting link
"The edge quality of holes also differs between drilling vs punching steel. Drilled holes typically have smooth edges and minimal burr formation. Punching, however, can produce rough edges and deformation zones around the hole perimeter."

Germany was doing whatever they could with the machine tools that hadn't been destroyed. I have a late war "Last Ditch" Mauser rifle bolt with all the machining marks clearly visible, showing how it was made.

"I forgot to include the other impediment mentioned. Germany was broaching, not milling, the aforementioned gears. From the above statement I gather that's less than optimum.

-----------------------------------

I believe that depends on how much the final tooth surface has been deformed and possibly cracked by the cutting force. Milling removes thin chips rapidly with little effect on the uncut metal while broaching may be a more brute force bulldozer approach, depending on the tooling and depth of cut.

----------------------------

Broaching isn't inherently worse, and may be a good choice for slots or splines within a hole. This is a broach set for cutting drive key slots in gear and pulley hub holes.

formatting link
? The step height between cutting edges is small and not damaging. I bought a few individual broaches for much less $$ and machine the round guide bushings as needed.

formatting link
"Gear design and materials: The Panther’s final-drive consisted of two cascaded spur-gear reduction sets driving the sprockets. This simple design (used because gear-cutting capacity for complex planetary gears was lacking) subjected gear teeth to very high contact stresses. German steel shortages meant gears had lower core strength and often lacked case hardening. Dr. Püschel (MAN) reported that fatigue of the intermediate gear – “due to the low-core strength of the material and the absence of case hardening” – caused most failures."

The original design specified planetary reduction gears which distribute the force among several gears.

formatting link

50 miles. It also consumed large quantities of gasoline; an always short critical resource.

---------------------------------

Additionally the British SOE sent an abrasive powder to sabotage the wheel bearings of the flatcars intended to transport the very dangerous 2nd SS Panzer Division to Normandy from central France, where they could move to oppose either a northern or southern invasion.

formatting link
March of Das Reich. Along the way they reacted to the Resistance the same way they had in Russia, weekly massacres. Germany sought needed cooperation from France and those responsible were scheduled for court-martial, though they died in the Normandy battles first.

formatting link
formatting link