Watched tank running day at Bovington (UK) FWIW

Sep 28, 2026 Last reply: 4 weeks ago 22 Replies
Jump to replies (22)

For what it's worth... went 2 days ago to Bovington camp tank museum for "running" day - of mainly WW2 armoured vehicles.



I can cite what I have studied about tanks. First time ever seeing tanks running. I set myself the goal of watching and absorbing...



Someone from the museum explained the cost in fuel (petrol/gasoline, diesel) runs into 5 figures GBPpounds (close to US$) *each day* - the admission cost from thousands of people barely covers.



Petrol/gasoline fueled tanks (the most) popping and banging away. Name of day heavily distorted by the only running WW2 German Tiger tank in the World (?) appearing. Heat-haze of gasoline being burned...



The amazing Soviet / Russian T34 (a T34/85) - one of very few diesel-engined tanks - blatantly displaying its crudity yet brilliance.



You folk are in the main experts. I will only comment - I am glad I saw. Seeing is understanding a lot...



Best wishes


For what it's worth... went 2 days ago to Bovington camp tank museum for "running" day - of mainly WW2 armoured vehicles.

I can cite what I have studied about tanks. First time ever seeing tanks running. I set myself the goal of watching and absorbing...

Someone from the museum explained the cost in fuel (petrol/gasoline, diesel) runs into 5 figures GBPpounds (close to US$) *each day* - the admission cost from thousands of people barely covers.

Petrol/gasoline fueled tanks (the most) popping and banging away. Name of day heavily distorted by the only running WW2 German Tiger tank in the World (?) appearing. Heat-haze of gasoline being burned...

The amazing Soviet / Russian T34 (a T34/85) - one of very few diesel-engined tanks - blatantly displaying its crudity yet brilliance.

You folk are in the main experts. I will only comment - I am glad I saw. Seeing is understanding a lot...

Best wishes

---------------------------------------

There are two tank museums about an hour from here in opposite directions. The operations manager of this one is a friend.

formatting link
have a live demo October 10 & 11.

I haven't visited this one yet.

formatting link
Tank driving was expensive and I hadn't been well coordinated driving a clutch and brake bulldozer so I settled for a half-track ride in the woods, which was like a roller coaster without seatbelts.

Being a motorhead I'd love to see the inner workings, some of which are visible in the tank repair shop demo.

formatting link
Their machine shop contained large, old, simple machine tools appropriate to WW2 tasks.

Bovington has a functional Tiger I and broken Tiger II, there's a running Tiger II in Saumur, France. As the war progressed bombing and lack of alloying metals cost German industry the ability to make adequately strong tank transmission gears, as well as stressed aero engine components.

formatting link
This was my usual ride in the Army because it had a safe to contain classified material. It was not much fun to drive, slow on the Autobahn and too wide for back roads.
formatting link
had Army versions of civilian vehicles such as the Suburban but no money for repairs when they broke. US forces in Europe were starved to support Vietnam. At least we could order Jeep parts privately from J.C.Whitney. Performance parts to make them faster also made them more likely to flip.

On a narrow winding back road in the Black Forest I had to drive my VW into the woods to avoid an oncoming convoy of British tanks. I took maximum advantage of knowing some German and being able to navigate my way around.

I also can't steer a tail-dragger plane with toe brakes, or leave a straight wake behind a sailboat. Maybe with more practice. I did learn to operate the four controls separately on a sliding dirt bike.

formatting link

For what it's worth... went 2 days ago to Bovington camp tank museum for "running" day - of mainly WW2 armoured vehicles.

-----------------------------------

In case you heard the argument that we were wrong to not adopt the Firefly modification, this explores the reasons. Mainly the Firefly was less accurate and less effective against infantry, the more common threat.

formatting link
"Where is the practical advantage to the capability to puch through at extended range if you can't get the shell to hit to begin with? By the time Firefly gets close enough to hit the target, [US Sherman] 76mm would be punching through as well anyway."

90mm refers to the larger gun on US tank destroyers.

I don't know how enthused you are, but there is a place here in the states where you can drive and even shoot tanks.

"DriveTanks.com

formatting link
and shoot real tanks! The World's premier living military history adventure. Experience the historic and rate anti-tank guns and machine guns."

Bovington has a functional Tiger I and broken Tiger II, there's a running Tiger II in Saumur, France. As the war progressed bombing and lack of alloying metals cost German industry the ability to make adequately strong tank transmission gears, as well as stressed aero engine components.

formatting link

--------------------------------

formatting link
Straight cut spur gears can be made on simple milling machines like mine while more complex geometries require rotating the gear blank in exact synchronization with the motion of the cutting tool. I've read that US daylight bombing that targeted vital factories significantly hurt German machine tool and war production manufacturing capability, as did the hydrogen peroxide aircraft and U-boot propulsion programs that robbed the rest of industry of already scarce nickel and other alloying metals. This book mentions the problem.
formatting link
A measure of the difference is that German aero engines needed half again the displacement to match the power of Allied engines.

That's actually a complex and controversial subject with each combatant having a different viewpoint that favors their capabilities and accomplishments.

-------------------------------

Impossible to park in civilian spaces, as at Autobahn rest stops. I liked the internal and external size of the 1970's VW camper van, but couldn't keep up with its road salt rust. That's why I've improved my ability to form sheet metal into repair panels and mig weld them.

The rivnuts are more trouble than expected because their heads space the patch outward on curves and shift the alignment of other holes. The Hardell tool doesn't reliably clinch 1/4-20 stainless rivnuts tight enough to not spin. Tightening a Gr8 bolt in them bottoms them out tight enough. I turned a sleeve bushing with a Vise-Grip handle to isolate the rivnut head from the rotational friction of the bolt head, then clean up the slightly deformed threads with a tap.

There are two styles of tools I am familiar with for setting rivet nuts. One that operates like a pop rivet tool, but it incorporates a threaded mandrel. Of those there ARE two sub types. A regular right angle fist grip tool of which most of us are familiar and a compound crimp tool with leverage more like a bolt cutter.

The other is simpler, may be cheaper (except at an industrial bolt supplier), and can be shop made. It is basically a GR8 bolt, a heavy washer, and a clearance fit hex fitting with a coarse knurl more like the bucking spikes on a chainsaw. You use a wrench on the hex with the spikes/knurl against the rivet nut, and tighten the bolt with a suitable wrench, socket, impact, or whatever. When the rivet nut is compressed in place you just back out the bolt.

I expect that one of these tools may work better than the others for your use. Some type or retaining compound might help. I don't know. I would also suggest if you are still enamored of the idea of rivet nuts, check to see if there are flush head countersunk versions available.

If a recessed or counter sunk head rivet nut is available some sort of dimple die might just be the ticket to make everything work the way you want.

Depending on how you punch the hole and dimple the sheet metal you may also be able to create increased engagement surface for knurling on the rivet nut itself.

There are two styles of tools I am familiar with for setting rivet nuts. One that operates like a pop rivet tool, but it incorporates a threaded mandrel. Of those there ARE two sub types. A regular right angle fist grip tool of which most of us are familiar and a compound crimp tool with leverage more like a bolt cutter.

The other is simpler, may be cheaper (except at an industrial bolt supplier), and can be shop made. It is basically a GR8 bolt, a heavy washer, and a clearance fit hex fitting with a coarse knurl more like the bucking spikes on a chainsaw. You use a wrench on the hex with the spikes/knurl against the rivet nut, and tighten the bolt with a suitable wrench, socket, impact, or whatever. When the rivet nut is compressed in place you just back out the bolt.

I expect that one of these tools may work better than the others for your use. Some type or retaining compound might help. I don't know. I would also suggest if you are still enamored of the idea of rivet nuts, check to see if there are flush head countersunk versions available.

If a recessed or counter sunk head rivet nut is available some sort of dimple die might just be the ticket to make everything work the way you want.

Depending on how you punch the hole and dimple the sheet metal you may also be able to create increased engagement surface for knurling on the rivet nut itself.

-- Bob La Londe CNC Molds N Stuff

---------------------------------

The Hardell tool is of the bolt cutter handle type which initially sets the rivnut without rotating it. I used my shop made bolt and wrench tool afterwards to pull the rivnut tighter, until I felt it bottom out. The initial set and the friction of the stationary sleeve bushing against the head were enough to keep the knurled stainless rivnut from turning from thread friction.

In this case the patch doesn't need to fit flush, a drainage gap may be better than sealing in high speed tire spray, which the original box channel design appears to have done on the V shaped and spotwelded bottom edge. I considered making a screw-together die set to form a shallow well around the rivnut head, but don't think it's appropriate or necessary on curved surfaces that it will distort, and 18 gauge galvy steel is difficult to simply shear or bend with a hammer. I've made such die sets for easier tasks like setting brass grommets in hanging tarps.

A more adjustable approach would be to fold the outer edges of the patch down to form a seal with some spring. I've found that with curved metal I need each forming operation to solve one problem without worsening another elsewhere.

Everything finally fits. I took it apart and sprayed LPS-3 inside the remaining box channel. The factory paint is still intact on exposed areas that I sprayed 20+ years ago.

Does anyone else take auto body repair to this level? I can buy repair panels for my 91 Ranger but not this 2000 Honda. I made the Ranger floor repair only because the available floor panel has the same drain hole where mine rusted around the rubber plug.

dimple die might just be the ticket to make everything work the way you want.

-- Bob La Londe

--------------------------

I made a dimpling die set for my #5 Junior punch. The limitation is access to the back side which a small rust hole or internal structure may not permit. My rust repairs to the truck and car have included Mig butt and plug welding when the back side is accessible to grind and spray, stainless pop rivets and auto body sealant, rivnuts for blind assembly and U clip nuts at edges. The non-welded patches are galvanized, the hardware stainless. The threads gall and stick together if not lubricated, LPS-3 which dries to a wax seems adequate so far. It's too thick to be a good grease for moving parts but it keeps them from seizing.

From my reading, the issue was lack of to harden the transmission ring gears, made worse by them broaching vs. milling them.

There was an edict against towing another tank because soon you had two dead tanks.

Allied knowledge of this lead to pre-D Day emphasis on taking out railroad lines along the Channel. This forced the Heer to road-march their armour instead. And on the later, heavier, tanks, roughly a third would have a transmission failure within

50 miles. It also consumed large quantities of gasoline; an always short critical resource.

From my reading, the issue was lack of to harden the transmission ring gears, made worse by them broaching vs. milling them.

There was an edict against towing another tank because soon you had two dead tanks.

Allied knowledge of this lead to pre-D Day emphasis on taking out railroad lines along the Channel. This forced the Heer to road-march their armour instead. And on the later, heavier, tanks, roughly a third would have a transmission failure within

50 miles. It also consumed large quantities of gasoline; an always short critical resource.

--------------------------------------

formatting link
“It is interesting that the American Sherman tank used double-herringbone gears in the final drives, which provides more torque capability for a given width of a final drive,” said Jacques Littlefield, founder of the Military Vehicle Technology Foundation, ...

His magnificent tank collection has passed to the American Heritage Museum.

Although gears require a slight clearance between mating teeth, on a herringbone gear the contact is continuous and moves across the faces. Straight cut spur gears jump and impact due to the clearance as the pressure passes between successive tooth pairs, adding to the force on them. Some older cars had straight cut reverse gears that were plainly louder due to the impacts than the more expensive herringbone forward gears.

Generally with angled teeth both the cutter and the blank have to rotate in synchronization on dedicated gear cutting machines.

Cutting straight across is much simpler, standard milling machines can do it with the addition of an indexer accessory to rotate the gear blank and hold it in each position. The cutter for both types is somewhat tricky to make but easy to sharpen by grinding the radial faces, which for an all steel gear cutter are where the yellow tungsten carbide inserts are in the picture. Tungsten carbide retains its sharp edge much longer than hardened tool steel.

formatting link
I've cut a custom gear for a repair by grinding the shape of one tooth space on the end of a lathe bit and rotating it like a fly cutter.

A few years ago on the local news they had an item about the energy crisis and showed a specialist gear cutter near Bristol UK cutting herringbone gears something similar to this

formatting link
, an energy intensive process so electricity prices effect them, IIRC our rate here is around 3x the US. I had never seen one in action before and didn't know how herringbone gears were made. I used to know a machinist that specialised in gear and spline cutting and had various Fellows gear shapers and other hobbing equipment so had seen the cutting of normal spur gears done on a Fellows shaper.

A few years ago on the local news they had an item about the energy crisis and showed a specialist gear cutter near Bristol UK cutting herringbone gears something similar to this

formatting link
, an energy intensive process so electricity prices effect them, IIRC our rate here is around 3x the US. I had never seen one in action before and didn't know how herringbone gears were made. I used to know a machinist that specialised in gear and spline cutting and had various Fellows gear shapers and other hobbing equipment so had seen the cutting of normal spur gears done on a Fellows shaper.

------------------------------ Thanks, I'd never seen that either. The gear cutting processes I looked into were older and suited to simpler general purpose machine tools like mine.

formatting link
The hard part is generating the cutting tool geometry, which is based on string unwinding from a spool at a constant speed. The contact between teeth duplicates the steady linear motion of a spot on the string. When translated to the string unwinding outward from a fixed spool that spot defines the tooth face curve.

There are shortcuts, for instance a gear of infinite diameter, a rack, has easily machined flat tooth faces. A cylindrical cutter shaped like an Acme thread can cut the correct tooth shape on a gear blank if angled so its teeth cut straight across while the blank rotates, either freely or synchronized.

formatting link

I've done the same to recut splines . Made an adapter to hold lathe cutters in my boring head ...

It looked like the cutter used to produce that herringbone gear was a rack profile so simple to produce. The Fellows cutters look like gears themselves so maybe a search is on for later to see how those are generated.

It looked like the cutter used to produce that herringbone gear was a rack profile so simple to produce. The Fellows cutters look like gears themselves so maybe a search is on for later to see how those are generated.

----------------------------------

One pre-CNC method I read of replaces the string on the spool with a flexible metal band that guides the cutting edge.

formatting link

I forgot to include the other impediment mentioned. Germany was broaching, not milling, the aforementioned gears. From the above statement I gather that's less than optimum.

Join the Discussion

Have something to add? Share your thoughts — no account required.

Didn't find your answer?

Ask the community — no account required