Anyone know of a more cost effective alternative to the TM2000 gas welding lens? THX, Ken
Alternative to TM2000 lens?
Jul 19, 2004
1 Replies
First reply
Gold Coated Cobalt Polycarbonate safety glasses. Around $35. guys also sell gold coated dydimium polycarbonate safety glasses thgat also work for aluminum gas welding. The gold-didies are more expensive. I have both and feel the cobalts work a little better, but both do work.
Read the full reply
Gold Coated Cobalt Polycarbonate safety glasses. Around $35.
formatting link
These guys also sell gold coated dydimium polycarbonate safety glasses thgat also work for aluminum gas welding.
The gold-didies are more expensive. I have both and feel the cobalts work a little better, but both do work.