Invertec V205-T with 7018 rod

Oct 03, 2003 0 Replies

>>> I would try >>>>increasing the arc force from 30 to 70% and see if >>>>that helps.

Made all the difference in the world. I would have thought the default setting would have been a little more usable. I was starting to think I had gotten to old and had lost my touch.


For the record I found that 50 -55% works.


Struggling with that low setting seems to have improved my welds. It was close to impossible to do any overhead work.