I have a Lincoln 175 SP Plus. It has a regulator that is in PSI, not cfm. I usually set it for 10 psi unless it's a little windy then 15. What do you use? Is that anywhere near correct?



Steve


You should get a "puff" of gas when your push the button/ and release it.

I have a flow meter on mine, with a pressure gauge.

My flow meter reads 15 cmf at 30psi.

Stick out when pressing the switch is about 3/8"

to much gas, you can see, welds aren't that good, to little gas, weld is difficult