I bought some tool steel that looks like that. I think it was "D-2" but I don't remember. However, I'll wager that it is hardenable tool steel.
Someone recommended a spark test. By comparing the spark glitter pattern to the pattern of known specimens you can come pretty close to determining what it is. I'll wager that it's high carbon of some kind. If so, for it to be weldable would imply pre- and/or post heat.
Vernon
Didn't find your answer? Ask the community — no account required.
I welded together a mobile base for a Bridgeport mill. (the castersare removable...
M
Mike Berger
B
brian458666
Since you have already contacted steel suppliers, and patiently searched "metal color codes" and similar terminology without finding your answers quit trying to ID it and do some experimenting to find useful properties. After all, this is not an engineering group where exact parameters need to be known.............. Brian
L
Lloyd E. Sponenburgh
Besides, Iggy.... who told you stainless steel wasn't (easily) weldable?
LLoyd
D
DoN. Nichols
It would have been nice if you had left quoted what I did about the actual color(s), to save me from having to follow the thread back and cut-and-paste it to an editor in a spare window before moving upstream again:
I've seen posted code charts from other vendors, and there was a
*lot* of difference. I think that difference is more common than similarity.
So -- now we dig into Jorgensen's book to see whether there is an actual match. What I *might* have to tell you is that it does not appear under that description in their book, but we'll see.
When two colors are mentioned, there is some of each visible, one over the other, so your "yellow and gray" description would not work there, and I can skip that if I find it.
And, I'll have to list "close" ones, since I can't see your bar in person.
Jalloy AR-360 heat treated bars brown
4140 annealed brown Type 303se, condition B brown Aluminum, 2011 brown
There is *no* mention of beige, or anything closer than brown.
There *is* a Yellow and gray, which is 1144 carbon steel
Most things in Jorgensen's book are bright primary colors to be harder to mistake. Nothing as light as a beige.
So -- it is someone else's code, not Jorgensen's.
Enjoy, DoN.
Join the Discussion
Have something to add? Share your thoughts — no account required.
Didn't find your answer?
Ask the community — no account required
Report Content
You are reporting this content to the moderators. They will look at it
ASAP.