I've been working on another boat project and looking through various manufacturers websites I've found that aluminum water pipe might be the best solution for one aspect. I want a 5052 pipe a wall thickness greater than the available tube I have found. Schedule water pipe seems to be a solution that exists. A few manufacturers do list it on their website, but I can't seem to find any "retail" at any of my usual sources. In fact very few seem to even have thin wall tube in 5052.



The first question some might ask is, "What's wrong with 6061? 6061 water pipe is available as is thicker wall 6061 tube." I want 5052 and



6061 isn't 5052. If I wanted to settle I would not need to make this post.

Cross posted to related groups only:



rec.crafts.metalworking rec.boats.building sci.engr.joining.welding


Diameter, schedule/wall thickness, length, total quantity?

I've been working on another boat project and looking through various manufacturers websites I've found that aluminum water pipe might be the best solution for one aspect. I want a 5052 pipe a wall thickness greater than the available tube I have found. Schedule water pipe seems to be a solution that exists. A few manufacturers do list it on their website, but I can't seem to find any "retail" at any of my usual sources. In fact very few seem to even have thin wall tube in 5052.

The first question some might ask is, "What's wrong with 6061? 6061 water pipe is available as is thicker wall 6061 tube." I want 5052 and

6061 isn't 5052. If I wanted to settle I would not need to make this post.

Cross posted to related groups only:

rec.crafts.metalworking rec.boats.building sci.engr.joining.welding

6061 isn't 5052. If I wanted to settle I would not need to make this post. >> >> Cross posted to related groups only: >> >> rec.crafts.metalworking >> rec.boats.building >> sci.engr.joining.welding > > Diameter, schedule/wall thickness, length, total quantity? >

Are you a vendor seeking to quote or do you know of a retail (online) source for 5052 aluminum pipe?

I've spent a bit of time looking and I think its as much what is available to me as it is what size I would really like. What I would really like is 5052 extrusions to fit the application, but what I have found to fit the application that is not proprietary is all 6061.

1-1/4 schedule 40 and 3/4 schedule 40. About 120 feet of each.

That would be some hellacious irrigation pipe. I've got a buddy who owns a several miles of irrigation pipe upto 12 inches. None of it is that thick.

I think its more likely it was cut from plate. There are even aluminum vendors who list circle (ring) cuts as standard order items on their websites.

formatting link

Not a vendor. Among other hats I wore at my last job I did a lot of the material purchasing for the machine shop and thought I'd maybe try some of the local vendors I used to deal with but I didn't know what to ask for. Doubt they will have anything other than 6061 in stock but thought it would be worth a phone call.

That would be some hellacious irrigation pipe. I've got a buddy who owns a several miles of irrigation pipe upto 12 inches. None of it is that thick.

I think its more likely it was cut from plate. There are even aluminum vendors who list circle (ring) cuts as standard order items on their websites.

formatting link

--------------------------

That's what I read, about the show's original props. The replicas seem to be cut from plate. I remember because I was surprised they would have pipe like that Down Under. Perhaps it carried water up into the New Zealand mountains where the show was filmed.

I burned through more than a day's internet ration looking for thick-walled tubing for hydraulics or to make deep submersible hulls. I have a use for

6063 T-1 rigid aluminum electrical conduit but I haven't found a local source.
formatting link