Welding machine-Tig info needed

Oct 21, 2006 5 Replies
Jump to replies (5)

I brought home today a Airco tig welder. It, except for the color..appears identical to the Miller Dialarc 250-HF.



Anyone know where I can find a manual and so forth? Ive not powered it up yet, just need to know how to set the HF points and so forth.



And yes..this is sorta a gloat. Ill find out if its a gloat or an Awshit later today when I put power to it and the chiller



Included Wp-20 torch, Miller pedal (looks new) and so forth.


Gunner


"A prudent man foresees the difficulties ahead and prepares for them; the simpleton goes blindly on and suffers the consequences."



- Proverbs 22:3


Congrats. I would keep the current setting, mine is 0.02", if I recall correctly.

i

I'm assuming youve checked the obvious

formatting link
If its been a pa> I brought home today a Airco tig welder. It, except for the

Ayup..found it right after I posted. Its been a very long week.

Oh..its a gloat. Works like a champ. Torch had a plugged passage, removed hoses, blew some air gently through in the reverse direction, blob of s*it came out. Not the usual Procon pump..not as high a pressure..shrug..but it puts out a fair stream. GOOD HF..ran about a

1/2" of HF on first push. This actually does a really nice job down at the low amp range..surprised me how stable it was all the way down at the near zero mark. Now Ill try welding two beer cans base to base...someday

"A prudent man foresees the difficulties ahead and prepares for them; the simpleton goes blindly on and suffers the consequences."

- Proverbs 22:3

I'm hopin' ya'll empty them first.... Ken.

Hold-my-beer-and-watch-this??