Wire difference

Jun 19, 2008 1 Replies

What is the difference between these two flux core wires?



E71T-11 Carbon-Steel E71T-GS


Well as best I can figure it...

E71T-11 has a lower hydrogen infusion level that E71T-GS, so unlike E71T-GS it CAN be used for multi-pass welds...BUT... It has no Charpie V Notch ratings so it is limited as to structural welding applications. For Structural work E71T-8 is preferred.

To equate these to stick rods... E71T-8 = 7018 Low Hydrogen, Structural. E71T-11 = 7014 Low Pen, clean , multi-pass for up to 1/2" steel E71T-GS = 6010 High pen, aggressive, single pass.