A coproduct of ethanol production could be used as a non-petroleum- based filler in plastics, based on preliminary studies by Agricultural Research Service (ARS) scientists and their cooperators. The ethanol coproduct, called distiller's dried grains with solubles (DDGS), has a high fiber content and a molecular structure suitable for binding=97two attributes that make it a candidate as a filler in plastics, according to ARS agricultural engineer Kurt Rosentrater.



Rosentrater is based at the ARS North Central Agricultural Research Laboratory in Brookings, S.D. He conducted the research with Robert A. Tatara, a professor at the Northern Illinois University (NIU) Department of Technology, part of NIU'S College of Engineering and Engineering Technology.



The researchers compressed molded blends of DDGS and phenolic plastic resin (ranging from 0 to 90 percent DDGS) and found that DDGS concentrations between 25 and 50 percent worked best as fillers in plastics. These findings were published recently in the Journal of Polymers and the Environment (JPE).



The preliminary study yielded only limited data on the resulting physical properties of the various DDGS/plastic blends, so follow-up tests are currently under way.



The data can then be used to develop new bio-based manufactured products. Rosentrater and Andrew W. Otieno, also with Northern Illinois University's Department of Technology, have developed comprehensive guidelines that take into account the unique challenges encountered when manufacturing plastic composites that contain biological materials. This work has also been published in the JPE.


Join the Discussion

Have something to add? Share your thoughts — no account required.

Didn't find your answer?

Ask the community — no account required