SWAAT Testing

Oct 31, 2005 0 Replies

Hi.



Anyone know where I can purchase the solutions to make up synthetic sea water for the SWAAT Corrosion Test in accordance with ASTM D1141. I am testing powdercoated Al coupons to ASTM G85:A3. UK agent or supplier preferred.



Cheers.



JJ