Cerium amount

Nov 22, 2004 1 Replies
Jump to replies (1)

Dear All,



I have difficulties to find labs which are able to deteremine the Cerium amount in Ni base alloy.



Does some has the experience on it ? Is there any lab that you know in UK or France or Germany



Is there other cost efective solution to analyse it other than OES



Thanks



Pierre


The problem you are having is many labs don't have cerium curves for ther OES's in a Ni-base matrix (probably due to lack of adequate standards). You may have better luck getting someone to do it by AA, again providing they have standards in the range your looking for.