The recent thread on gas bottles prompts this question...
I have a bottle of CO2 and another of Argon. And a bottle of O2 for that matter. If I wanted to try blends is there a mixing device made? Or, has somebody built their own? From what I've read this would mostly benefit MIG welding.
Karl
Didn't find your answer? Ask the community — no account required.
It's the wrong fitting for straight CO2, they usually use the CGA320that...
D
dcaster
Do some searches on Sci.engr.joining.welding. Ernie has posted info on the mixer he put together from parts. Mixing would also help TIG, but you would need to invest in a Helium bottle. Ernie likes to add some helium to the argon when welding thick aluminum.
=20 Dan
P
Pete C.
I believe Ernie has posted about gas mixers before on sci.engr.joining.welding and I think there may be something about it on his stagesmith site.
W
Woodworker88
The welder who does alot of my work has a commercial manifold/mixer on his TIG setup, with Argon, Helium, and Nitrogen coming in, and lines running to his TIG torch and two more outlets for back-gassing various parts. All you really need is a regulator and flow gauge for every tank, some piping, and a way to purge everything as needed. Since you're doing everything at low pressure (the regulator goes right on the tank), you can use standard pipe parts.
If I built one of these, I'd spend a little extra money and buy new regulators that all had identical shapes and markings, to reduce the chance of making a mistake when setting up the mixture.
Join the Discussion
Have something to add? Share your thoughts — no account required.
Didn't find your answer?
Ask the community — no account required
Report Content
You are reporting this content to the moderators. They will look at it
ASAP.