replying to Ignoramus29878, Jeff l wrote: Yes you can use a tig welder to melt precious metals. You need a crucible with a carbon ground added to the bottom to complete the circuit. A closed box similar to a sandblasting cabinet is helpful. You flood it with argon prior to your melt to further protect the metals. Look up James Binnion. He uses this process with incredible success mixing/melting karat golds, platinum, palladium, silver etc. He uses it to make mokume gane rings etc. The results are second to none. Look for his video doing it. I am getting ready to try it myself