Compatability Issue

Jun 17, 2005 2 Replies
Jump to replies (2)

Right then my second problem in as many days. I'm in the process of making cherry dice cups/pots for a gaming group that I attend. I shall be finishing the edges with 1/4" brass angle. Because of the name of the group I want to put a copper plate 1 3/4" x



1 3/4" on the lid held down with the brass angle. This plate will be engraved with a Gryphon. Now I've heard some strange rumours about brass, copper and various reactions to other material. Is it OK to use these three together (Brass, copper and cherry) without causing discolouration? And if it is OK what's the best way to protect both the wood and metal after the lids return from the engravers.

I'm used to carpentry and apart from screws & nails I rarely ever use metalwork.



Many Thanks for any advice.



TR



I think you should look up the phrase, "galvanic corrosion" on Google. I could be wrong, but I think this is the problem you're worried about...

Regards,

Robin

I don't think you will have any problems. Copper and Brass are pretty close on the electrochemical series.

Dan