Andrew Mawson

"Ignoramus32654" wrote in message news:PB%tf.3904$H% whether No need for copper - a steel plate works fine but will be sacrificed over time. I've seen people say don't use stainless steel as that makes for an environmentally nasty electrolyte to dispose of. AWEM

Read the full reply

I have certain copper pieces that I could use as electrodes for EDR. I am not sure if that is safe from environmental standpoint and whether copper would dissolve (I may later use them for different purposes). Any ideas?



i

whether

No need for copper - a steel plate works fine but will be sacrificed over time. I've seen people say don't use stainless steel as that makes for an environmentally nasty electrolyte to dispose of.

AWEM

I see.. Thanks. I have plenty of junk steel that is leftovers from my welding practice. I will simply stick to it.