Being a bear of very little brain and less skill I come asking for help.
I have to drill a hole in a strip of steel, so far so good, I can manage that.
But I then have to countersink it, a thing I've never done before.
Do I need a special bit or can I do it with a large drillbit?
Is there a special technique such as go more slowly than normal or go faster than normal? Should I size the larger bit exactly to the head of the countersunk bolt or should it be larger?
Zebee
Didn't find your answer? Ask the community — no account required.
[ ... ] [ ... ] Hmm ... I *think* that we've got a problem of mixed units. ...
L
limeylew
The best way would be to use a 'countersink bit' but it also depends to some extent on how thick the material is and how 'professional' do you want it to look.
For most situation it will be best to use a slower speed than what you drilled with.
Hope this will help you.
Lewis.
*****
B
Bruce In Bangkok
If you want the countersink to fit anything then you need to use a countersink bit, which also has more then two cutting edges and in addition to cutting the correct angle is more likely to make a smooth cut.
By the way, wood screws have an included angle on the head of 82 degrees, machine screws have an included angle of 82 degrees, but rivets have a 78 or 100 degree included angle. You will need to match the countersink to the fastener used. Cheers,
Bruce (bruceinbangkokatgmaildotcom)
D
David Billington
IIRC the 82 degree coutnersink angle is used for unified screws, metric and BSF, BSW use 90 degree countersinks so the OP needs to check what is being used.
R
Richard Edwards
Also note that metric countersunk screws have an included angle of 90 degrees upto and including M20 thereafter 60 degrees! (Source Unbrako Eng guide) I must admit that until fairly recently I did not appreciate that UNC UNF etc were 82 degree inc angle not 90.
Richard
B
Bruce In Bangkok
Many, many different angles but none of them are the 118 degrees of a standard drill bit..... :-) Cheers,
Bruce (bruceinbangkokatgmaildotcom)
D
Don Foreman
formatting link
Low speed works best for me.
S
spaco
Just to add a little more complexity:
I have been countersinking holes with a standard drill bit that's about
3 times the diameter of the hole. This works for me because I am using (mostly) 1/16" diameter mild steel rivets in the holes and manually riveting them in place. So, I am forming the material to fit the countersunk hole as I go. In this application, I don't need a lot of strength so the thin head that results from the 118° angle isn't a problem.
You can see this application at:
formatting link
As the other posters have said, go buy a set of appropriate countersinks. They will last a long time and will eventually add to the value of the estate sale.
Pete Stanaitis
---------------
J
Jim Wilkins
Find one that is rated for steel, not just wood.
jw.
G
Gunner Asch
And hold the piece of steel very very securely. Preferably with a clamp on a drill press.
The problem with using a larger bit to countersink..and we all do it..is if the metal workpiece is too thin..its easy to blow right through if the drill bit gets a good bite and screws itself through the metal. With a drill press, you can control the "bite", as long as the metal is held down so its not pulled into the drill bit.
If all you have is a hand drill motor...brace yourself well and go Slow! when applying pressure, and turn the bit slower.
My $,02USD worth of opinion
Gunner
"First Law of Leftist Debate The more you present a leftist with factual evidence that is counter to his preconceived world view and the more difficult it becomes for him to refute it without losing face the chance of him calling you a racist, bigot, homophobe approaches infinity.
This is despite the thread you are in having not mentioned race or sexual preference in any way that is relevant to the subject." Grey Ghost
B
Bob Engelhardt
The best countersinks I've ever used are the "through hole" style. /Never/ any chatter.
formatting link
of the page.
Bob
Z
Zebee Johnstone
Thanks heaps for the information. Looks like I need to find a suitable countersink bit for a 5mm bolt.
Buy more tools. Oh the horror!
Hrm... why, when I have had way too much time on my hands for the last
3 weeks do I need to find a bit, some 5mm Nyloks, and some ethernet cable (not related, but still required) in a window of around 2 hours on Saturday morning?
Zebee
B
Bill Noble
snip----------
WRONG!!! - machine screws are available with 90 or 82 degree angle, the 90 deg is used for thinner material
B
Bruce In Bangkok
Not to dispute you but I'll bet if you stroll over to either Walmart or Harbour Freight, as so many on this group apparently do, you will get 82 degree heads.... Cheers,
Bruce (bruceinbangkokatgmaildotcom)
S
Stealth Pilot
use a slocombe drill of the appropriate size in a drill press.
you 'merkins will probably swear blind that they are called centre drills.
Stealth Pilot
S
Stealth Pilot
huuuuuuuuunnneeeeeeeeyyyyyyy its been 3 weeks now and my widget still isnt fixed. no nookies for you until it gets fixed.
:-)
Stealth Pilot
R
Randall Replogle
Don't you get chatter from the two flutes? I get the best results with a single flute cs. I've ever had much luck with multiple flute ones. RR
D
DoN. Nichols
No Harbour Freight in reach, and I don't patronize Walmart, but I would not expect anything but the most basic screws there.
I know that I have some 90 degree and some 82 degree screws, and probably some other angles as well. Granted that some of these were left-overs from a job building flight simulators with standard aviation style hardware.
It was where I learned about Clecos and Rivnuts, among other things.
Enjoy, DoN.
D
DoN. Nichols
Well ... center drills (we would never spell them "*centre* drills") have a 60 degree angle, to match the angle on lathe centers. And I would not normally consider them for countersinking screws.
I've got the 82 degree and the 90 degree countersinks in several styles and sizes -- as well as 180 degree ones (normally called "counterbores". :-)
Enjoy, DoN.
D
DoN. Nichols
The multi-flute ones like the Severance ones (with slightly staggered flutes) I find it best to bring the drill press spindle and countersink down into firm contact with the workpiece before switching on the motor.
Enjoy, DoN.
P
P D Fritz
For accurate countersinking you need the proper countersinking bit and a tool that can be adjusted for the proper depth of cut. Since countersinking is very common with various aircraft parts, aviation machinists commonly use the tools shown in this catalog to precisely control the depth of the cutting bit.
formatting link
Join the Discussion
Have something to add? Share your thoughts — no account required.
Didn't find your answer?
Ask the community — no account required
Report Content
You are reporting this content to the moderators. They will look at it
ASAP.