I have stripped out the threads in a 1/4" bolt hole in an aluminum transmission case. I can't get a drill in there to be able to use a heli-coil type of insert, and I have decided to use JB Weld to repair this as the bolt that goes into this stripped hole just locates a bracket which is held on securely by another, larger bolt. I haven't used JB Weld before, but I am confident this is an appropriate situation to try it...
I checked out the website where it tells me to clean with acetone, no problem. My question is how to proceed from there, assuming that I want to be able to remove and replace the bolt after it cures.
Do I just force the epoxy mix into the hole and then jam the bolt in ? Or should I coat the bolt with oil so the JB Weld doesn't bond to it? I am worried that if I don't do something, when I unbolt the bolt, it might pull the whole wad of epoxy out instead of unscrewing.
Thanx for not telling me not to strip out bolt holes in aluminum, I already know that this is a bad thing!