what is it?

Aug 07, 2003 6 Replies

First reply

Dave Baker

It looks like the needle valve in the float chamber of a carburetor so I suspect it performed the same function in a restricting valve in a pipeline. The deformation will have taken place primarily in the seating area below the tip where the fluid velocity is highest. Bernoulli…

Read the full reply

At this site you will find a picture of a focault pendulum clock that has a cone shaped piece of metal from a hydroelectric generating station. nThe metal is 'said' to be really hard, but it has been abraded/contorted into a very interesting shape. The question is....what part is it, what was it's function? It is interesting to note that the very tip shows little deformation/abrasion; could it be the 'end' instead of the 'point' of an apparatus in the flow of water? rick



formatting link


It looks like the needle valve in the float chamber of a carburetor so I suspect it performed the same function in a restricting valve in a pipeline. The deformation will have taken place primarily in the seating area below the tip where the fluid velocity is highest. Bernoulli would have us believe the pressure falls as the velocity increases so I suspect that at high flow rates the fluid was cavitating there leading to the interesting shapes worn into the metal.

Dave Baker - Puma Race Engines

formatting link
I'm not at all sure why women like men. We're argumentative, childish, unsociable and extremely unappealing naked. I'm quite grateful they do though.

I think it is the exhaust cone on a water turbine, It's purpose is to reduce cavitations ? bill k

Neat picture... the deformation is almost certainly due to cavitation. Cavitation damage is like having a lot of little explosions at the surface of the part.

Tim.

I've got a book on cavitation and cavitational wear, that's definitely cavitational damage. My off the cuff guess would be that it was part of the nozzle assembly on the turbine, I've seen drawings of similar cones hooked to the turbine governers, they move axially in and out of the nozzle to throttle the water flow. It's amazing what moving water can do to metal, isn't it?

Stan

didn't some once said that water was the universal solvent!

What size particles are you talking about in the errosion process? By that I mean what would be the average particle size of the metal as it leaves the surface of the cone? rick