All all 7018 rods created equal?

Sep 07, 2003 21 Replies

I have found that the Lincoln rods of late aren't the same as they used to be. I've had much better luck with ESAB. The Lincoln rods have a H4 on them - fresh out of the can and right into an oven. Very hard to use at lower amps - and too much heat with more amps.

I'm not sure that is just the rods as I've been using a Invertec V205-T to do this stick welding.

Could it be the V205-T? Miller claims on their new dynasty 200DX that is is a better stick welder than the V205-T.

Has anyone used both with 7018 rod?

Can anyone give me a comparison: Dynasty 200DX vs Invertec V205-T on

7018 rods (5/32).

Haven't run any 7018 on the Invertec, but it runs really smooth on my Maxstar 200DX.

Join the Discussion

Have something to add? Share your thoughts — no account required.

Didn't find your answer?

Ask the community — no account required