Brazing - Do You Prefer TIG or OA?

Feb 09, 2005 2 Replies

First reply

Ernie Leimkuhler

I much prefer TIG Braze Welding, but it is a different animal than gas brazing. "Braze welding" denotes an actual bronze bead, while "brazing" denotes a flowed joint with no real bead.

Read the full reply

For those who have used both TIG and OA for brazing, which do you prefer (i.e. which do you find easier, more useful)? TIA



I much prefer TIG Braze Welding, but it is a different animal than gas brazing. "Braze welding" denotes an actual bronze bead, while "brazing" denotes a flowed joint with no real bead.

You're the expert, Ernie, but a flux-gas braze joint looks great when your done.