filler for 5052 and 6063

Apr 21, 2004 2 Replies
Jump to replies (2)

What is the best filler for welding 5052-h32 sheet 0.1" thick to 6063-t52 angle 0.125" thick with a Square Wave 175 tig



Thanks.


5356 or for a little more strength, 5556.

Thanks for the quick response. I will give it a try.

Join the Discussion