Material is S45C or C45.



It is recommended by the customer that after forging (at min850+10=B0C), it must fall in quenching tank with polymer quenching system.



but we can't be sure that all forging will be at the same or in



850+10=B0C temp when fall in to quenching media.

we propose, forging will be re-heated at 860=B0C in our Continuous furnace and will be quenched at 860=B0C+10=B0C 9 or 850=B0C+10=B0C in the tank. in this way we can maintain exactly same temp before quenching and all forgings will have same micro structure and hardness. But customer is not agreeing, saying that micro structure obtained thus will cause problem to machining which is very minute and precise.



I just wonder how come micro same micro structure, which obtained through different process will affect machining.