Re: Best gas for a 110V Mig ?

Aug 23, 2003 0 Replies


Just wondering what is the best gas for a 110V MIG welder. I got the


>Craftsman one from Sears that I am pretty sure is made by Century as it >looks the same.
>What is the best gas ? Also, I have a small CO2 tank form my younger years
>when I had a Keg fridge inside the house. Would this CO2 and tank work for a
>setup ? It isn't a syphon tank but I don't know if you would want to use one
>of them anyhow for welding.
>
>Thanks,
>Iowa883
>
>
>

Your CO2 tank will work ok with MIG welder. If your shielding gas regulator starts freezing on cold days hang incadesent light on it to heat.