building trailer axles

Mar 29, 2021 0 Replies

I am tring to replace old mobile home axle with mismatched barings. Looks like my best choice is to customer make them. What steel should be used for



6,000/7,000lb axles? Would 3" OD x 0.25 = 2.5" ID in ERW, HRW, BW, DOM with a little heat be able to slip over the SP-25042 axles (2.5" OD)? Or would I have to freeze (dry ice) the axle also? One place list 3"x7/32 wall at 2.562" ID in ERW & DOM, would that be a better option & strong enough, still waiting on a price?

Standard #42 spindels (3,500 b each) SP-22542 = 2.25" OD, SP-25042 = *2.50" OD* Standard brake mounting plates are 2-1/2" ID or *3-1/8" ID*


Join the Discussion

Have something to add? Share your thoughts — no account required.

Didn't find your answer?