supply oil tempered steel wire

Sep 22, 2013 0 Replies

Commodity: Oil tempered irregular steel wire



  1. Material JIS: SUP6; SUP7; SUP9; SUP9A; SUP10; SUP12; SUP12V; S60C. SAE: SAE9254; SAE9260; SAE6150; SAE9255; SAE9254V; SAE1566; SAE1065. DIN: 55Cr3; 60Si7; CK67; 60SiCr7; 50CrV4; 100Cr6.
  2. Usage Suspension spring; auto stabilizer bar; household appliances; furniture manufacturing; auto and motorcycle parts; electronic appliances; etc.
  3. Size According to customer's requirement.
  4. Material chemical composition

see more detail :

formatting link