Most of you are probably aware of the basic idea of liquid thread locking compounds.



"Red" - High strength for medium to larger bolts most people will run across.



"Blue" - Medium strength for the mid size and smaller bolts most people will run across.



Until I ran across needs that was about the limit of what I knew. I expect most non professional mechanically inclined people start there.



The next one I ran across was "Green" which was a sleeve and bearing locker. I used it on a "press" fit hose fitting on a pickup truck engine I was working on. Probably in my early 20s.



Then later I discovered "Purple" which is a light thread locker. I used it on fishing reel components I still wanted to be able to get apart without heating up small parts that probably can't take the heat not even accounting for plastic parts nearby.



Then I started learning that the colors were just a rough guide, and that there were various formulas for special applications. Steam fittings, thread sealers, etc. Yes, still talking about "thread lockers" formulations here.



A while back I was working on an air rifle (real small game power) which use a pair of set screw to restrict airflow and regulate power. One was turned into a hole that crossed the air passage until reaching the desired power/velocity, and the other back stopped the first to "lock" it in place. The back stop didn't always work. The answer was VC3 from Vibratite. Its a non locking thread locker. Its supposed to prevent a a screw (or other threaded item) from moving from vibration, but allow it to move using a tool and not need to be reapplied for many cycles. It was perfect for dialing in that air gun flow restricter. Then I just set it and forget it. I did gently put in the back stop screw, but the VC3 kept the screw in place through a few days of adjusting and tweaking to get just the power and velocity I was looking for.



On my big (for me) manual mill (10x54 table, 5hp, 16x36 travels) I almost never use the dials on the hand wheels, but they have threaded collars that snug them in place when using them. Less damaging I suppose than set screws, but they have a problem. They back off on their own over time. I've gone so far as to snug them down with a pair of slip joint pliers. I find them to be awkward and in the way sometimes. On the knee it activates the safety switch and prevents me from powering up or down the knee. I don't want to get rid of them, because I do know how to machine using the hand wheels and not that long ago one of my DRO scales flaked out. I had to use the hand wheels to do some work until I fixed the DRO.



Do you think a couple drops of VC3 on the threads of those locking collars would be a good idea?



I'm not sure how much force would be required to move them, but I suppose I could drill a hole, and use a spanner if its more than my hand strength. The spanner for my keyless chuck (which is always right there) might be made to work.



On a Bridgeport with a DRO I use it instead, of course. I've found that I can approach, slow and stop at the dimension faster on the Clausing because I can read the moving stamped numbers on the dial more easily than the blur on the DRO.

That wasn't the question.

That wasn't the question.

Well, I decided to try it. 3 drops 120 degrees apart on each of the 4 threaded locking collars. (2 on the table, 1 on the saddle, and 1 on the knee) It might be a while since I very rarely use the dials, but when I find out I'll let you all know how smart or how stupid it was. Anybody know how long it takes VC3 to cure?

There's a dial integrated with my power feed on the mill , also held by a lock ring . I've never had mine come loose . I rarely refer to it since I upgraded my DRO .

<snip>

They suggest 30 minutes for most applications:

formatting link
I bought a couple tubes awhile back but haven't used it yet. It's one of those items you need NOW and don't want to stop what you're doing to go buy it...

Join the Discussion

Have something to add? Share your thoughts — no account required.

Didn't find your answer?

Ask the community — no account required