Killing a cylinder

Feb 24, 2014 1 Replies
Jump to replies (1)

I have an old 300 O2 cylinder I want to saw the bottom off, and make a noisemaker cannon. Someone said that the local steel people would saw it off for cheap or free. Anyone have any experience? Or can I just flood it, and torch it?



Steve


You do not need to flood it. Just empty it, keep the valve open, and torch it.

Any shop with a big enough bandsaw could do it for you.

i

Join the Discussion

Have something to add? Share your thoughts — no account required.

Didn't find your answer?

Ask the community — no account required