Anyone has an idea how to weld together Titanium pipe 1/2" dia with a copper sleeve or tube???
Titanium vs copper welding
Dec 08, 2003
1 Replies
Anyone has an idea how to weld together Titanium pipe 1/2" dia with a copper sleeve or tube???
Brazing, not welding, would probably work.
Josh
Pierre Giass> =