Any special preparation / jigging?
Welding exhaust manifolds?
Jan 13, 2004
1 Replies
First reply
assuming cast iron there is a process of pre/post heating that must be followed to prevent further stress fractures. see get you started.
Read the full reply
assuming cast iron there is a process of pre/post heating that must be followed to prevent further stress fractures.
see
formatting link
get you started.