Apr 26, 2005 0 Replies

We are the manufacture factory of polycarbonate film and sheet in China. The thickness range is from 0.125mm ~1.0mm. Our standard grades as below are very competitive both in price and quality around world market.



Polycarbonate film: OM-G11 polished/polished (same like Lexan8010) OM-G42 velvet/matte (same like Lexan8b35)



PC film with different transparent color



Thickness: 0.125, 0.175, 0.25, 0.3, 0.38, 0.5, 0.78, 0.8, 1.0 (mm)



Standard Width: 915mm, 927mm, 930mm, 1000mm



This is the website of our company:

formatting link
. And there are our brief introduction and products information on it. The quality of our film is good, please consider about it. If you have interesting about our film, we also can send some samples for you with the data sheet of our products. Expecting for your reply.. Best regards..



Sophia Bao Suzhou OMAY Optical Material Co.,Ltd Huashan Road 158-30#, Suzhou , Jiangsu , China 215011 Tel: +86-512-66652011 H/P: +86-13382182015 Fax: +86-512-66652012 Email: snipped-for-privacy@pc-film.com