A few more pictures of the Larios as it goes back together

Jan 03, 2010 5 Replies
Jump to replies (5)

formatting link
Final paint tommorow..all the trim work, then set all the covers and finish the electrical.



Gunner



"I am for doing good to the poor, but I differ in opinion of the means. I think the best way of doing good to the poor, is not making them easy in poverty, but leading or driving them out of it. In my youth I travelled much, and I observed in different countries, that the more public provisions were made for the poor the less they provided for themselves, and of course became poorer. And, on the contrary, the less was done for them, the more they did for themselves, and became richer." -- Benjamin Franklin, /The Encouragement of Idleness/, 1766


Gunner, What do you use to do the derusting? Why wouldn't you clean up the rust BEFORE you paint? Steve

you paint?

I used a wire wheel and a phosphoric acid liquid to "kill" any remaining rust that I couldnt get.

Using a good tough wire wheel to get off any flaking paint and thick rust. and then the rust killer does a pretty good job,.and means I dont have to dig deep and then putty the gouges back up before painting

After wire wheeling, I used mineral spirts to get any dust and oils and grease, then brushed on a coat of the phosphoric acid solution, waited an hour..then was ready to paint.

Gunner

"I am for doing good to the poor, but I differ in opinion of the means. I think the best way of doing good to the poor, is not making them easy in poverty, but leading or driving them out of it. In my youth I travelled much, and I observed in different countries, that the more public provisions were made for the poor the less they provided for themselves, and of course became poorer. And, on the contrary, the less was done for them, the more they did for themselves, and became richer." -- Benjamin Franklin, /The Encouragement of Idleness/, 1766

I think you may have misunderstood the question or I misunderstood your answer. I meant the machined surfaces not the paint prep. Steve

you paint?

I meant the machined surfaces not the paint prep.

Oh! It was only a light surface rust and I did clean it up before painting. Are you concerned that its dark colored? Thats the result of the phosphoric acid making the rust turn almost a black color. Which was then wire brushed, and then treated with the acid again. Im not a fan of Shiney..so left the last treatment of acid turn the steel black. The phosphoric acid is part of the treatment for Parkerizing as well as other metal treatings.

The last thing I want is a "shiney bright silver" table on any mill. Shrug..just a personal choice...chuckle..and it hides future stains and light rust better

Gunner

BEFORE you paint?

"I am for doing good to the poor, but I differ in opinion of the means. I think the best way of doing good to the poor, is not making them easy in poverty, but leading or driving them out of it. In my youth I travelled much, and I observed in different countries, that the more public provisions were made for the poor the less they provided for themselves, and of course became poorer. And, on the contrary, the less was done for them, the more they did for themselves, and became richer." -- Benjamin Franklin, /The Encouragement of Idleness/, 1766

answer. I meant the machined surfaces not the paint prep.

I used Oxpho-Blue on the ways of my Atlas 618 for much the same effect.

David