Metal identification reference online

Oct 01, 2003 1 Replies
Jump to replies (1)

formatting link
Air Force Technical Manual: CONSERVATION AND SEGREGATION OF CRITICAL ALLOY AND PRECIOUS METAL BEARING PARTS AND SCRAP.



Great info! Classifications, spark tests, density tests, acid tests, AISI- AMS-PWA cross-references.