You can buy custom-assembled Ni-Cd batteries from Digi-Key. You basically select any of the standard cells, and then specify the pattern the cells should be stacked in, and how many cells you need. They go for very roughly $10 a set.
Jon
You can buy custom-assembled Ni-Cd batteries from Digi-Key. You basically select any of the standard cells, and then specify the pattern the cells should be stacked in, and how many cells you need. They go for very roughly $10 a set. Jon
Read the full reply
You can buy custom-assembled Ni-Cd batteries from Digi-Key. You basically select any of the standard cells, and then specify the pattern the cells should be stacked in, and how many cells you need. They go for very roughly $10 a set.
Jon
I'm trying to adapt an older portable air-band scanner receiver and a cheap FM transmitter to provide airport CTAF chatter on an FM frequency so that people sitting in the parking lot of our airport can tune in on their car radios and listen. This scanner forgets the frequency it was tuned to if turned off without a battery inside, so I need to provide a good battery for backup if AC power is lost. The radio was originally designed for NiCAD batteries, and provides a simple series resistor to charge the battery. Can NiMH batteries be charged this way? NiMH battery chargers seem to be more sophisticated than the usual NiCAD (DC) chargers. Nevertheless, I suspect that a simple series resistor will provide what I need, although I will need to change to a higher resistor to just keep a trickle charge on the batteries. Anyone know if you can continuously trickle charge NiMH batteries, which are now much easier to obtain than NiCADs? Thanks for any help you experts can provide.
-- Bob (Chief Pilot, White Knuckle Airways)
Nickel-metal-hydride batteries don't like extended trickle charging, and recommended trickle-charge rate is half that of nickel-cadmiums: 0.05C rather than 0.10C.
Here's a good source for basic charging info. Look around the site; you'll find most of what you want to know:
-- Ed Huntress
In general NiMH would not be a good choice for backup use unless you have a pretty sophistocated charging system. They are great for high draw evices like portable CD players and cameras because they maintain voltage to the very end but they self discharge pretty rapidly so they are not good for things like emergency flashlights that get used infrequently but need to work when needed.
Yes.
In general - maximum life expectancy can be expected if a dedictaed charger meant for each battery chemitry is used.
The optimum charge methon is that NiCd are charged at maximum allowed current (with a temperature moninor if possible) until their battery voltage peaks and then starts to drop (ie voltage dropping even though charging is going on)
NiMH need to have charge termination earlier - one needs to stop charging when battery voltage remains constant during charging.
Continuous tricle charging will be tricky, as if the batteries are charged excessively, their performance and life expectancy will suffer.
If you have any electronics background - do a search 9or call)
Here is a great link with lots of good information about batteries, chemistries and charging methods etc.
And another
Have something to add? Share your thoughts — no account required.