OT - "Static Cling" in printer paper?

Jan 10, 2005 4 Replies

First reply

Jim Stewart

In the very early days of copy machines, we were instructed to 'fan' the ream of paper before putting it in the paper tray. Just grab the edge of the long end of the ream and wave it around letting the sheets slide across one another.

Read the full reply

SWMBO just pulled me down to her office (It's at the opposite end of our office suite from mine, works great for both of us that way. ) to comlain that her laser printer "wasn't working". (Samsung ML 1430)



Sure enuf, it went through the motions but wasn't picking up a piece of paper from the sheaf sticking out of the paper slot.



After peering down the slot while it tried to do it's thing I diagnosed it as a glazed eccentric rubber paper pickup roller and spent about twenty minutes disassembling the printer far enough so I could get in and swab that roller off with acetone.



Damn thing didn't work any better except there was a noticable chirp from the pickup roller when it tried to slide the "top" sheet of paper off the sheaf.



That's when I woke up and realized I couldn't slide one sheet of paper off either, even when I gave my finger a lick first.



Grabbed a different ream of the same brand of paper - no problemo.



Just thought I'd mention that to help someone else who may experience a similar problem. MProbably due the winter weater and the fact that there's no humidification in the buildings HVAC system.



I tried fixing the "bad" sheaf of paper by taking one sheet at a time off the stack and huffing on it. When I piled up about twenty of them so treated the printer fed them all fine.



Jeff


In the very early days of copy machines, we were instructed to 'fan' the ream of paper before putting it in the paper tray.

Just grab the edge of the long end of the ream and wave it around letting the sheets slide across one another.

I was told to "break" the ream open by bending it around a corner for the same reason. Pat

Another technique is to press the knuckle of your middle finger against the ream and execute a one inch circular motion until the ream fans out. Kind of neat to watch.

Regards,

Boris Mohar

Got Knock? - see: Viatrack Printed Circuit Designs (among other things)

formatting link

The paper needs 'fanning'.

In a 'previous life' I maintained all the photocopiers and offset printers in a community college and paper jams/non-feeds were a daily problem. It took me a long time to 'educate' the users on the correct paper loading techniques but once they 'got it' my work load was reduced considerably ;-).

The 'packs' of paper you buy are actually guillotined out of a much larger block. During this process the edges of the paper can 'lock' together almost like microscopic 'velcro'. When you open a new pack you

*must* break the bonds *before* putting it into the printer/photocopier.

There are several ways of doing this but all of them work.

1) Grasp one short side firmly and use your thumb to slide down the opposite edge forcing the paper to 'jump apart'. Repeat from the other side then re-stack the paper by gently tapping the pack on a flat surface on the long and short sides and load.

2) Grasp a corner and do the above.

3) Grasp diagonally opposite corners and gently bend the pack back and forth while applying a gentle 'forward' pressure with one thumb and a 'backward' pressure with the other thumb. The pack should start to rotate and break the bonds. Continue until all the pack has started to turn and no sections of paper are still stuck together then re-stack the paper by gently tapping the pack on a flat surface on the long and short sides and load.

Most paper packs also have printed information saying which way is 'up'. Usually when you split open the wrapping the paper facing you is the 'top' of the pack. It helps the feeding process if you keep that orientation intact when you load it into the printer/copier.

One of the other major causes of jamming/feed problems is sudden changes in humidity. High humidity causes the paper to swell which leads to binding problems in the very 'tight' spaces it passes through on its way through the machine.

HTH.

Join the Discussion

Have something to add? Share your thoughts — no account required.

Didn't find your answer?

Ask the community — no account required