Have a question?

Sep 16, 2003 1 Replies
Jump to replies (1)

I recently purchased a used Miller Dialarc 250 stick welder.



I also have a Bobcat 250NT which came with a FC3195 wire feeder.



My question is can I use the wire feeder with the Dialarc? I think so but would like some input before smoking something.



thanks in advance.


OOPs..

Should have been 3045FC wire feeder.....

Sorry.

Join the Discussion

Have something to add? Share your thoughts — no account required.

Didn't find your answer?

Ask the community — no account required