Would like to know what tri-mix is good for this application. I have He 18% Co2 4% balance Ar, but have seen others. I don't do a lot of this welding so would like your opinion.



Thanks Richard


That looks like a standard tri-mix. Should work fine. You will need to up your voltage a tad for stainless since the SS wire is a very poor conductor. Also keep your wire stickout extremely short.