Ready Welder and TIG/Stick source.

Oct 20, 2003 1 Replies
Jump to replies (1)

This question is mostly directed at Ernie, (because I know he uses a Ready Welder with an inverter(?) setup), but someone else here might have an answer. I have a chance to buy a 10250 ready welder, and I'm thinking of getting it so I can run a MIG setup for those few times it would be handy for me. My existing machine is a Lincoln Squarewave 275, which should work fine (on DC) according to what Ready welder says. Anyone know of any issues with this setup? I can't see why it would hurt the Squarewave or the ready welder, but it's possible I'm missing something.......



Pete


Should be fine. If you want to use 0.024" wire in the Readywelder to weld 18 ga or 16 ga steel sheet or tube, use the arc control setting on the machine to reduce the open-circuit voltage.

Join the Discussion

Have something to add? Share your thoughts — no account required.

Didn't find your answer?

Ask the community — no account required