Welding aircraft tubing book

Aug 21, 2005 2 Replies
Jump to replies (2)

Found this book on the EAA site Aircraft Welding

formatting link
There is also one available on ebay item # 4570139084



John


sent too fast; found a second book on ebay item # 4569641368 Building the custom aircraft with welding published by the EAA 1970's edition

John

Thanks for this. I snagged it and it's got some neat tricks for working with tubing. Cool stuff.

Peter