Jun 27, 2005 1 Replies
Jump to replies (1)

Question.



What are some realistic settings for a good (32 or better) sidewall finish in 6061 Al with... say a 1/2" cutter. DOC, anywhere from 1X to



3X.

Machine has a 10k spindle and is 2.5 years old.



How much of a factor is the holder? Can you crank up the RPM and adjust the IPM accordingly?



Thank you,



Peter.



You own a better machine than I've ever ran....

For that good a finish with that DOC side milling; lots o' luck. Of course, try high rpm, climb mill, very sharp tool, flood coolant, adjust feed for a sweet spot. You might try posting over on alt.machines.cnc