Lubricants for Taft Peirce Surface Grinder?

Sep 06, 2008 2 Replies
Jump to replies (2)

What lubricants should be used on an ancient Taft-Peirce 5 x 12 manual surface grinder? It does have a Bijur pump on the side.



Thanks for any help.



Chuck


For the ways, Vactra #2 available from McMaster Carr.

Wes