⏣ General Metalworking

30778 Threads Posts
to

Amorphous steel

What do you guys know or hear about amorphous steel? Supposedly they add the element yttrium and it keeps the steel from...
8 comments posted 21yrs
posted by bamboo
8 comments posted 21yrs posted by bamboo

OT: Midsize Backhoe Loader Advice wanted

Going to do some building in a fairly remote area. Toying with the idea of buying a mid sized backhoe/loader. Something...
5 comments posted 21yrs
posted by escarcegaNOSPAM
5 comments posted 21yrs posted by escarcegaNOSPAM

Honda ad

Gang, My son sent me this link - http://www.stlplaces.com/honda.htmla Honda commercial (which may or may not have aired...
12 comments posted 21yrs
posted by Ken Sterling
12 comments posted 21yrs posted by Ken Sterling

Another tool ID needed XXIII

Just posted a few more photos, I have no idea what number 196 is for: http://puzzlephotos.blogspot.com/
34 comments posted 21yrs
posted by rhvp65
34 comments posted 21yrs posted by rhvp65

Making square holes in thick Aluminum Plate

Gentlemen, Hope you are fine wherever you may be. I have a job which came my way which calls for making 2"x2" square ho...
12 comments posted 21yrs
posted by richard.mcbride7
12 comments posted 21yrs posted by richard.mcbride7

To shaper or not to shaper ?

Ok, $200 for a shaper of question but probably decent quality. $600 to ship. I know absolutely nothing about shapers bu...
3 comments posted 21yrs
posted by no
3 comments posted 21yrs posted by no

Making Gold Solder from Scraps

Hi :-) This is Heather in England, been on this group a few times in the past with a few questions... here's a new one....
10 comments posted 21yrs
posted by heather
10 comments posted 21yrs posted by heather

Damaged Aluminum Rims

I just purchased aluminum rims that were damaged on the lip. Would it be possible to weld a lip back on it? The chip is...
18 comments posted 21yrs
posted by steve_cornick
18 comments posted 21yrs posted by steve_cornick

Help requested for NC tape drive

We recently acquired a Newing-Hall 'Pantocut' light milling machine and engraver. It has an NC control unit and program...
4 comments posted 21yrs
posted by diesel
4 comments posted 21yrs posted by diesel

Craftsman tools not warranted/guaranteed forever

Today I tried to return my Craftsman clicker /ratchet torque wrench for a replacement because the lock-unlock switch is...
65 comments posted 21yrs
posted by jfladd
65 comments posted 21yrs posted by jfladd

Rigger's nightmare

For your interest and edification, I present the following link: Jim
59 comments posted 21yrs
posted by jim_member
59 comments posted 21yrs posted by jim_member

Brazing band saw blades

To those that have 'em broken and/or have difficulties obtaining right width/teeth/composition in required length: you...
3 comments posted 21yrs
posted by rashidk
3 comments posted 21yrs posted by rashidk

Slotting (milling) aluminum - the answer

A while back I posted some questions on the subject. In general the responses to my and prior questions were not too go...
8 comments posted 21yrs
posted by rashidk
8 comments posted 21yrs posted by rashidk