1K epoxy system

Hi,

I wnt to formuate1k Epoxy system which gets cured at 50-60 celcius. can anyone help with the curing system.

Thank you

Gaurang Thosani dgc snipped-for-privacy@rediffmail.com

Reply to
bipin thosani
Loading thread data ...

Hi,

I wnt to formuate1k Epoxy system which gets cured at 50-60 celcius. can anyone help with the curing system.

Thank you

Gaurang Thosani dgc snipped-for-privacy@rediffmail.com

Reply to
bipin thosani

That's too cool for heat curing. Your best bet is to use a traditional amine curing agent. Check out Cognis's Versamid curing agents. EV Roberts will sell them in small quantities (1 qt.). Versamid 140 works well and will cure with bisphenol A diglycidyl ether in approximately 30 minutes at that temperature.

Reply to
bjr

Vers_amid_ are polyamide curing agents.

Then it will also cure at RT in a few days and you will not get a very useful 1K epoxy system.

Regards, Oliver

Reply to
Oliver 'Ojo' Bedford